ALKAN M., Andreev D., SÖNMEZ M. Ş. , Sanin V., Yukhvid V., DERİN C. B. , ...More
XIII International Symposium on Self-Propagating High-Temperature Synthesis, Antalya, Turkey, 12 - 15 October 2015, pp.72
-
Publication Type:
Conference Paper / Summary Text
-
City:
Antalya
-
Country:
Turkey
-
Page Numbers:
pp.72