EURO CERAMICS VIII, PTS 1-3, ss.395-398, 2004 (SCI-Expanded)
Nano-composite sol-gel coatings on commercial glasses were applied by dip coating. Coating solution contained TEOS and GLYMO together with solvent, water and acid as a catalyst. Withdrawing rates of 2, 6 and 12 inch/min were applied and heat-treatment conditions were 200degreesC for I hour in static air.